Abstract
Acid mine drainage occurs when sulfide minerals are exposed to an oxidizing environment. The objective of this study was to inhibit the oxidation of pyrite by applying various coating agent such as KH2PO4, MgO and KMnO4 over its surface as an oxidation inhibitors. Experiments were conducted for 8 days to test the feasibility of oxidation inhibitors. The optimal condition of coating agent for standard pyrite and IK mine was the combination of 0.01M KH2PO4, 0.01M NaOAc and 0.01M NaClO. Otherwise, for YD mine the combination of 0.01M KMnO4, 0.01M NaOAc and 0.01M NaClO. The SO42− reduction efficiency of pyrite, IK and YD mine samples was 70, 92 and 84%, respectively. For 8 days, no significant increase of SO42− from pyrite sample coated with inhibitor was observed. The pH of solution remains in between 4 to 6 for the reaction conditions.
URI
http://pubs.kist.re.kr/handle/201004/38209
ISSN
1598-6438
Appears in Collections:
KIST Publication > Article
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML


qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE