<?xml version="1.0" encoding="utf-8" standalone="no"?>
<dublin_core schema="dc">
<dcvalue element="contributor" qualifier="author">Jung,&#x20;Woo&#x20;Sang</dcvalue>
<dcvalue element="contributor" qualifier="author">Han,&#x20;Sungsoo</dcvalue>
<dcvalue element="contributor" qualifier="author">Kim&#x20;Dong-Ik</dcvalue>
<dcvalue element="contributor" qualifier="author">SHIM,&#x20;JAE-HYEOK</dcvalue>
<dcvalue element="contributor" qualifier="author">SEUNG&#x20;CHEOL,&#x20;LEE</dcvalue>
<dcvalue element="date" qualifier="accessioned">2024-01-13T02:30:48Z</dcvalue>
<dcvalue element="date" qualifier="available">2024-01-13T02:30:48Z</dcvalue>
<dcvalue element="date" qualifier="created">2021-09-29</dcvalue>
<dcvalue element="date" qualifier="issued">2009-04</dcvalue>
<dcvalue element="identifier" qualifier="uri">https:&#x2F;&#x2F;pubs.kist.re.kr&#x2F;handle&#x2F;201004&#x2F;101407</dcvalue>
<dcvalue element="subject" qualifier="none">High&#x20;strength&#x20;steel</dcvalue>
<dcvalue element="subject" qualifier="none">Ab-initio&#x20;calculation</dcvalue>
<dcvalue element="subject" qualifier="none">Nucleation</dcvalue>
<dcvalue element="subject" qualifier="none">(TiMo)C&#x20;carbides</dcvalue>
<dcvalue element="subject" qualifier="none">Thermo-mechanical&#x20;treatment</dcvalue>
<dcvalue element="title" qualifier="none">TiC&#x20;강화&#x20;고강도강의&#x20;핵생성&#x20;및&#x20;석출강화&#x20;기구</dcvalue>
<dcvalue element="type" qualifier="none">Conference</dcvalue>
<dcvalue element="description" qualifier="journalClass">2</dcvalue>
<dcvalue element="identifier" qualifier="bibliographicCitation">2009년도&#x20;대한금속재료학회&#x20;춘계학술대회,&#x20;복합상&#x2F;나노입자제어형&#x20;기가철강소재&#x20;심포지움,&#x20;pp.92</dcvalue>
<dcvalue element="citation" qualifier="title">2009년도&#x20;대한금속재료학회&#x20;춘계학술대회,&#x20;복합상&#x2F;나노입자제어형&#x20;기가철강소재&#x20;심포지움</dcvalue>
<dcvalue element="citation" qualifier="startPage">92</dcvalue>
<dcvalue element="citation" qualifier="endPage">92</dcvalue>
<dcvalue element="citation" qualifier="conferencePlace">KO</dcvalue>
</dublin_core>