<dcvalue element="contributor" qualifier="author">김항종</dcvalue>
<dcvalue element="contributor" qualifier="author">LEE&#x20;SUN&#x20;KYUNG</dcvalue>
<dcvalue element="contributor" qualifier="author">오태성</dcvalue>
<dcvalue element="contributor" qualifier="author">HYUN&#x20;DOW&#x20;BIN</dcvalue>
<dcvalue element="date" qualifier="accessioned">2024-01-13T18:33:16Z</dcvalue>
<dcvalue element="date" qualifier="available">2024-01-13T18:33:16Z</dcvalue>
<dcvalue element="date" qualifier="created">2021-09-29</dcvalue>
<dcvalue element="identifier" qualifier="uri">https:&#x2F;&#x2F;pubs.kist.re.kr&#x2F;handle&#x2F;201004&#x2F;110096</dcvalue>
<dcvalue element="language" qualifier="none">English</dcvalue>
<dcvalue element="subject" qualifier="none">bismuth&#x20;telluride</dcvalue>
<dcvalue element="title" qualifier="none">Thermoelectric&#x20;properties&#x20;of&#x20;the&#x20;hot-pressed&#x20;Bi2(Te,Se)3&#x20;alloys&#x20;with&#x20;the&#x20;Bi2Se3&#x20;content&#x20;and&#x20;addition&#x20;of&#x20;scattering&#x20;center</dcvalue>
<dcvalue element="type" qualifier="none">Conference</dcvalue>
<dcvalue element="description" qualifier="journalClass">1</dcvalue>
<dcvalue element="identifier" qualifier="bibliographicCitation">Proceedings&#x20;of&#x20;the&#x20;17th&#x20;International&#x20;Conference&#x20;on&#x20;Thermoelectrics,&#x20;pp.174&#x20;-&#x20;177</dcvalue>
<dcvalue element="citation" qualifier="title">Proceedings&#x20;of&#x20;the&#x20;17th&#x20;International&#x20;Conference&#x20;on&#x20;Thermoelectrics</dcvalue>
<dcvalue element="citation" qualifier="startPage">174</dcvalue>
<dcvalue element="citation" qualifier="endPage">177</dcvalue>
<dcvalue element="citation" qualifier="conferencePlace">JA</dcvalue>
</dublin_core>