Water deoxygenation using a hollow fiber membrane contactor to prevent pipe corrosion for sustainable management of district heating systems: A pilot-scale study

Authors
Lee, JihoBaek, Soo-MinBoo, ChanheeSon, AseomJung, HoseokPark, Sung SooHong, Seok Won
Issue Date
2020-12
Publisher
ELSEVIER SCI LTD
Citation
JOURNAL OF CLEANER PRODUCTION, v.277
Abstract
Dissolved oxygen (DO) is a key factor affecting pipe corrosion in district heating systems (DHS). This study demonstrated effective deoxygenation of water in a DHS using a hollow fiber membrane contactor (HFMC) via systematic investigation from lab-to pilot-scale. First, deoxygenation efficiency was evaluated in a lab-scale HFMC with varying operating parameters including an effective membrane area, flow rate and feedwater temperature. Based on the results from the lab-scale investigation, a pilot HFMC system was designed with capacity of 1 m(3) per day. To achieve a permeate DO concentration below 10 mu g L-1 at feedwater temperatures of 20-60 degrees C, the vacuum degree needed to be lower than the saturated water vapor pressure of 10-120 Torr. In addition, the primary foulant for membrane fouling was organic matter in the make-up and district heating (DH) return water. A significant change in corrosion response was observed for pipe steel in the DHS after deoxygenation. Immersion tests for 14 days indicated that weight loss values had greatly reduced by the deoxygenation process from 39.3 to 1.3 mg cm(-2) and from 21.9 to 2.1 mg cm(-2) for steel pipe samples immersed in the make-up water and the DH return water of the DHS, respectively. This improved corrosion resistance from deoxygenation was interpreted by electrochemical analysis. As such, this study offers a pilot-scale demonstration of the feasibility of a hollow fiber membrane-based deoxygenation process as an effective tool to prevent the corrosion of steel pipes. (C) 2020 Elsevier Ltd. All rights reserved.
Keywords
DISSOLVED-OXYGEN; ULTRAPURE WATER; TEMPERATURE; REMOVAL; DESIGN; OXIDE; District heating system; Deoxygenation process; Corrosion; Hollow fiber membrane
ISSN
0959-6526
URI
https://pubs.kist.re.kr/handle/201004/117749
DOI
10.1016/j.jclepro.2020.124049
Appears in Collections:
KIST Article > 2020
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE