Cobalt oxide co-doping effect on the sinterability and electrical conductivity of nano-crystalline Gd-doped ceria
- Authors
- Prasad, D. Hari; Park, S. Y.; Ji, H.; Kim, H. -R.; Son, J. -W.; Kim, B. -K.; Lee, H. -W.; Lee, J. -H.
- Issue Date
- 2012-01
- Publisher
- ELSEVIER SCI LTD
- Citation
- CERAMICS INTERNATIONAL, v.38, pp.S497 - S500
- Abstract
- Nano-crystalline 3 mol% CoO-doped GDC (Ce0.9Gd0.1O1.95) powders of high sinterability at lower sintering temperature have been synthesized by deposition-precipitation method. The physical and chemical properties of the obtained powders were characterized by XRD, XPS, BET, EDS and TEM. From sintering studies, CoO-doped GDC can be fully densified (97% relative density) at a lower temperature of 850 degrees C. It has also been found that the sintered samples have a higher ionic conductivity of 2.38 x 10(-2) S cm(-1) at 600 degrees C in air. (C) 2011 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
- Keywords
- GRAIN-GROWTH; MICROSTRUCTURE; POWDERS; GRAIN-GROWTH; MICROSTRUCTURE; POWDERS; Powders: chemical preparation; Electrical conductivity; CeO2; Fuel cells
- ISSN
- 0272-8842
- URI
- https://pubs.kist.re.kr/handle/201004/129685
- DOI
- 10.1016/j.ceramint.2011.05.062
- Appears in Collections:
- KIST Article > 2012
- Files in This Item:
There are no files associated with this item.
- Export
- RIS (EndNote)
- XLS (Excel)
- XML
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.