Synthesis of a Cr2AlC-Ti2AlC ternary carbide

Authors
Kim, Chang-SamHwang, Sung IkHa, Jung-SooKang, Seung-MinCheong, Deock-Soo
Issue Date
2010-02
Publisher
KOREAN ASSOC CRYSTAL GROWTH, INC
Citation
JOURNAL OF CERAMIC PROCESSING RESEARCH, v.11, no.1, pp.82 - 85
Abstract
The Cr2AlC ternary carbide is excellent in chemical and oxidation resistances as well as mechanical properties at high temperatures. Therefore it satisfies most requirements for as an interconnector Material in solid oxide fuel cells (SOFCs). However, its thermal expansion coefficient is higher than those of the anode and cathode so that a high thermal stress is generated unavoidably between them during heating and cooling SOFCs. Thus we attempted to reduce the thermal expansion coefficient through a solid solution with Ti2AlC which has a lower thermal expansion coefficient. Dense and single phase (Cr1-xTix)(2)AlC solid solutions with a relative density of 99.5% or more were synthesized by hot pressing a mixture of CrCx, Ti2C, Al powders at 1250 degrees C for 4 h. The limitation of Ti substitution was found to be less than 20 mol%. When Ti substitution exceeded this limit, unreacted Ti2C, Cr7C3, and Cr3C2 remained as second phases. The grain size decreased with Ti substitution. With 5 mol% Ti substitution, the thermal expansion coefficient could be lowered by 5% compared with the case without substitution in the temperature range of 700-800 degrees C.
Keywords
MECHANICAL-PROPERTIES; OXIDATION; CR2ALC; 1300-DEGREES-C; TI3SIC2; MECHANICAL-PROPERTIES; OXIDATION; CR2ALC; 1300-DEGREES-C; TI3SIC2; Cr2AlC; Ti2AlC; solid solution; thermal expansion coefficient; oxidation resistance
ISSN
1229-9162
URI
https://pubs.kist.re.kr/handle/201004/131764
Appears in Collections:
KIST Article > 2010
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE