Research on the surface oxidation procedure of Fe-base metallic glass during wet oxidation treatment

Authors
Kang, Eun YoungChung, Young HoonOk, Myoung-RyulBaik, Hong Koo
Issue Date
2007-03-25
Publisher
ELSEVIER SCIENCE SA
Citation
MATERIALS SCIENCE AND ENGINEERING A-STRUCTURAL MATERIALS PROPERTIES MICROSTRUCTURE AND PROCESSING, v.449, pp.159 - 164
Abstract
Internal structure of magnetic core for high-frequency use could be divided into small insulating units to minimize eddy current loss. Accordingly, the powder size of Febal.Si9.6B14.4Nb4 (numbers indicate at.%) amorphous alloy should be small and covered with some degree of insulating layer for producing high-frequency magnetic core. In this investigation, formation of the insulating layer on the surface of Fe-based amorphous alloy powder was studied using wet oxidation method. The size of Fe-Si-B-Nb amorphous alloy powder used in this research was less than 75 mu m in diameter. Forming mechanism of surface cracks and consecutive oxide layers was explained and the thickness of insulating layer could be controlled by changing treatment time and concentration of HNO3 in the oxidizing solution. Even though the oxide layer on the powder surface was partially flaked off during hot-compacting process, sufficient electrical resistance was maintained to lessen eddy current loss effectively. (c) 2006 Published by Elsevier B.V.
Keywords
ALLOYS; ALLOYS; Fe-Si-B-Nb amorphous powder; surface oxidation; insulating coating; magnetic core; core loss
ISSN
0921-5093
URI
https://pubs.kist.re.kr/handle/201004/134522
DOI
10.1016/j.msea.2006.02.311
Appears in Collections:
KIST Article > 2007
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE