Abstract
A possibility to produce microwave (MW) dielectric materials by liquid-phase sintering of fine particles was investigated. Zn3Nb2O8 powders with a grain size 50-300 nm were obtained by the thermal decomposition of freeze-dried Zn-Nb hydroxides or frozen oxalate solutions. The crystallization of Zn3Nb2O8 from amorphous decomposition products was often accompanied by the simultaneous formation of ZnNb2O6. Maximum sintering activity was observed for single-phase crystalline Zn3Nb2O8 powders obtained at the lowest temperature. The sintering of as-obtained powders with CuO-V2O5 sintering aids results in producing MW dielectric ceramics with a density 93%-97% of the theoretical, and a Q x f product up to 36 000 GHz at sintering temperature (T-s)>= 680 degrees C. The high level of MW dielectric properties of ceramics was ensured by intensive grain growth during the densification and the thermal processing of ceramics.
Keywords
MICROWAVE DIELECTRIC-PROPERTIES; THERMAL-DECOMPOSITION; NIOBATES; V2O5; ADDITIVES; MN; NB; MICROWAVE DIELECTRIC-PROPERTIES; THERMAL-DECOMPOSITION; NIOBATES; V2O5; ADDITIVES; MN; NB; Microwave dielectrics; Freeze drying; Sintering aids; LTCC; Precipitation
ISSN
0002-7820
URI
https://pubs.kist.re.kr/handle/201004/134997
DOI
10.1111/j.1551-2916.2006.01246.x
Appears in Collections:
KIST Article > 2006
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE