Effect of preheating temperature of multiplex-type slurry cup on the morphology of primary solid phase of semi-solid slurry
- Authors
- Kang, Suk-Won; Lee, Dock-Young; Kim, Ki-Bae
- Issue Date
- 2006-09
- Publisher
- TRANS TECH PUBLICATIONS LTD
- Citation
- SEMI-SOLID PROCESSING OF ALLOYS AND COMPOSITES, v.116-117, pp.332 - 335
- Abstract
- Semi-solid slurry for a rheocasting process requires a fine and globular structure of primary solid phase. In the present study, in order to find an optimum preheating temperature of a multiplex-type slurry cup in the slurry maker that we recently developed for the rheocasting process, the semi-solid slurry was held for a various time of up to 60 min. in a multiplex-type slurry cup preheated at a different temperature. A size and morphology of primary solid phase of the semisolid slurry was measured and analyzed with the difference of the recorded cooling curve during the solidification with respect to a preheating temperature of the slurry cup. Also, a microstructural evolution and globularization mechanism occurred during the isothermal holding were discussed. Finally, as considering the effect of a different casting condition on the morphology of primary solid phase the optimum manufacturing condition of the semi-solid slurry for the rheocasting process was proposed.
- Keywords
- ALLOYS; STATE; ALLOYS; STATE; semi-solid slurry; primary solid phase; a preheating temperature of slurry cup; globularization; isothermal holding
- ISSN
- 1012-0394
- URI
- https://pubs.kist.re.kr/handle/201004/135177
- DOI
- 10.4028/www.scientific.net/SSP.116-117.332
- Appears in Collections:
- KIST Article > 2006
- Files in This Item:
There are no files associated with this item.
- Export
- RIS (EndNote)
- XLS (Excel)
- XML
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.