Optimization of foaming process using triblock polyimides with thermally labile blocks

Authors
Kim, DWHwang, SSHong, SMYoo, HOHong, SP
Issue Date
2001-01
Publisher
ELSEVIER SCI LTD
Citation
POLYMER, v.42, no.1, pp.83 - 92
Abstract
Triblock polyamic acid was synthesized from the reaction of amine-terminated polystyrene with 4,4'-oxydianiline and pyromellitic dianhydride in N-methyl-2-pyrrolidone. IR and TGA were used to determine optimum curing conditions, in which imidization was completed and the thermally labile polystyrene block was intact. From the thermomechanical analysis (TMA), it was identified that the resulting triblock polyimide film showed contraction at several points over the temperature range of 50-400 degrees C. The first contraction at 75 degrees C and the second at 275 degrees C were due to the residual stresses associated with the polystyrene and polyimide blocks, respectively. The third at 330 degrees C was probably attributed to foam collapse. The structural instability in polyimide matrix induced by the residual stresses was believed to be the reason causing the foam collapse. To overcome such a problem, an annealing process was carried out. The annealed film showed no contraction and, moreover, no foam collapse was observed in the thermomechanical analysis. (C) 2000 Elsevier Science Ltd. All rights reserved.
Keywords
SPONTANEOUS MOLECULAR-ORIENTATION; RESIDUAL-STRESS; THIN-FILMS; IMIDIZATION; TEMPERATURE; NANOFOAMS; COPOLYMERS; HISTORY; SPONTANEOUS MOLECULAR-ORIENTATION; RESIDUAL-STRESS; THIN-FILMS; IMIDIZATION; TEMPERATURE; NANOFOAMS; COPOLYMERS; HISTORY; triblock polyimide; thermomechanical analysis; foam collapse
ISSN
0032-3861
URI
https://pubs.kist.re.kr/handle/201004/140804
DOI
10.1016/S0032-3861(00)00026-4
Appears in Collections:
KIST Article > 2001
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE