Spin wave excitation on amorphous Co(80+x)TM(12)B(8-x) alloys
- Authors
- Yu, SC; Han, SM; Kim, KY; Noh, TH
- Issue Date
- 1996-05
- Publisher
- ELSEVIER SCIENCE BV
- Citation
- JOURNAL OF MAGNETISM AND MAGNETIC MATERIALS, v.157, pp.237 - 238
- Abstract
- Amorphous Co(80+x)TM(12)B(8-x) (TM = Ti, Zr, Hf, Nh; x = 0, 2, 4 at%) alloys were prepared by the single-roller melt-spinning technique. The saturation magnetization of the amorphous ribbons was measured by a SQUID and a vibrating sample magnetometer at 5-800 K under an applied field of 10 kOe. Typical thermo-magnetization curves were observed, and average values of the spectroscopic splitting g factor were estimated from the ferromagnetic resonance (FMR) curve. For all the amorphous alloys studied here, the saturation magnetization in the temperature range 5 K up to about 0.3T(C) can be described by the Bloch relation, M(s)(T) = M(s)(0)(1 - BT3/2 - CT5/2). The spin wave stiffness constants were calculated from the values of M(s)(0), B and the spectroscopic splitting g factor.
- Keywords
- spin wave excitation; amorphous; spectroscopic splitting factor
- ISSN
- 0304-8853
- URI
- https://pubs.kist.re.kr/handle/201004/144450
- DOI
- 10.1016/0304-8853(95)01227-3
- Appears in Collections:
- KIST Article > Others
- Files in This Item:
There are no files associated with this item.
- Export
- RIS (EndNote)
- XLS (Excel)
- XML
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.