MAGNETIC-PROPERTIES OF (CO93CR7)-P-PT/CR THIN-FILMS FOR LONGITUDINAL MAGNETIC RECORDING MEDIA

Authors
SOHN, HKSEOL, SCKANG, TSHIN, KHLEE, TDJANG, PW
Issue Date
1994-11
Publisher
IEEE-INST ELECTRICAL ELECTRONICS ENGINEERS INC
Citation
IEEE TRANSACTIONS ON MAGNETICS, v.30, no.6, pp.4041 - 4043
Abstract
We report here (Co93Cr7)-P-Pt thin films with the coercivity higher than 2600 Oe at the thickness of 180 Angstrom (M(r).t value of 0.9 memu/cm(2)) even when they were deposited without substrate heating and bias voltage. The effects of the film composition and the magnetic layer thickness were studied. The coercivity of Co-Cr-Pt film increased with addition of P up to 12 at. %. With addition of P, the degree of Co (0002) texture was reduced and the grain size of films became more uniform. These effects appear to be associated with the coercivity increase.
Keywords
DENSITY; DENSITY
ISSN
0018-9464
URI
https://pubs.kist.re.kr/handle/201004/145463
DOI
10.1109/20.333983
Appears in Collections:
KIST Article > Others
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE