2000-07 | A comparison of mechanical properties of all-ceramic alumina dental crowns prepared from aqueous- and non-aqueous-based tape casting | 김대준; 이명현; 이득용; 한중석 |
2000-12 | A new manufacturing method of all ceramic restoration using alumina tape and presentation of clinical cases | 오남식; 김의성; 이근우; 한중석; 김대준; 이명현 |
1997-01 | A simplified phase diagra in the ternary system Y2O3-Ta(Nb)2O5-ZrO2 | 이득용; 김대준; 장주웅; 이명현 |
1985-01 | A study of corrosion-resistant materials for pulsed gaseous core nuclear system. | 김대준; E. D. Whitney; D. S. Tucker |
2000-11 | Aqueous-based alumina tape casting | 이명현; 박일석; 김대준; 이득용 |
1999-01 | Bond valence anlysis of tetragonal zirconias | B. A. Hunter; C. J. Howard; 김대준 |
1993-01 | Characterization of Screen Printed YBa₂Cu₃Ox Thick Films | 김태윤; 김승구; 김대준; 현상훈; 정형진 |
2000-06 | Chromaticity, hydrothermal stability, and mechanical properties of r-ZrO₂/Al₂O₃ composites doped with yttrium, niobium, and ferric oxides | 이득용; 김대준; 송요승 |
1999-01 | Complex modulus of alumina green tapes measured by micro fourier rheometer | 이정훈; 이명현; 김창은; 김대준; Michael V. Swain; Bruno Pfister |
1995-01 | Determination of solid solubility limit of GeO//2 in 2 mol% Y//2O//3-stabilized tetragonal ZrO//2 by raman spectroscopy. | 김대준; 장주웅; 정형진; 허진우; 양인상 |
2002-02 | Dispersion and rheological characteristics of alumina slurries in aqueous tape-casting using acrylate binder | 조유정; 박일석; 문주호; 김대준 |
1994-01 | Effect of alloying on raman spectra of tetragonal zirconia. | 김대준; J. W. Jang |
2001-10 | Effect of alumina particle size on R-curve behavior of (Y,Nb)-TZP/Al₂O₃ composites | 이득용; 김대준; 김배연; 송요승 |
2000-04 | Effect of Fe₂O₃ addition on mechanical and optical properties of t-ZrO₂/Al₂O₃ composites | 이득용; 김대준; 이명현; 박일석; 최현 |
1993-01 | Effect of Nb//2O//5 alloying on thermal expansion anisotropy of 2 mol% Y//2O//3-stabilized tetragonal ZrO//2. | 김대준; P. F. Becher; C. R. Hubbard |
1998-10 | Effect of Nb//2O//5 and Y//2O//3 alloying on the mechanical properties of TZP ceramics | Deuk Yong Lee; 김대준; Duk Ho Cho; Myung-Hyun Lee |
1998-01 | Effect of organic additive composition on glass transition temperatures and storage moduli of Al2O3 green tapes | 이명현; 이정훈; 김창은; 김대준; 오남식 |
2000-08 | Effect of organic additive composition on lsostatic thermocompression behavior of alumina tapes | 이명현; 박일석; 김대준; 이득용 |
1993-01 | Effect of surface Grinding on Low Temperature Degradation of 3Y-TZP | 김대준; 이홍림; 정형진 |
1990-01 | Effect of Ta//2O//5, Nb//2O//5 and HfO//2 alloying on transformability of Y//2O//3-stabilized tetragonal ZrO//2. | 김대준 |
1992-01 | Effect of Ta₂O5 Alloying on Low Temperature Degradation of 3 mol% Y-TZP | 김대준; 최두진 |
1997-01 | Effect of tetravalent dopants on Raman spectra of tetragonal zirconia | 김대준; 장주웅; 이홍림 |
1994-01 | Effective ionic radius of Y3+ determined from lattice parameters of fluorite-type HfO2 and ZrO2 solid solutions. | 김대준; S. H. Hyun; S. G. Kim; M. Yashima |
2002-04 | Electrical conductivity of ZrO₂ doped with Sc₂O₃ and CeO₂ | 이동석; 허장원; 김재동; 김주선; 이해원; 김긍호; 김대준; 이종호 |
2003-07 | Evaluation of ceramic hip joint heads | 김대준; 김신윤; 최헌진 |
1997-01 | Fabrication of in-cream core by sheet forming process | 김대준; 이명현; 김장은 |
2001-11 | Fabrication of water-based ceramic tapes using PVP as binder | 박일석; 조유정; 이명현; 최세영; 이득용; 김대준 |
2001-01 | Flaw tolerance of (Y,Nb)-TZP/Al₂O₃ composites | 이득용; 김대준; 이명현; 장주웅 |
1998-01 | Fracture toughness, ionic conductivity, and low-temperature phase stability of tetragonal zirconia codoped with yttria and niobium oxide | 김대준; 정형진; 장주웅; 이홍림 |
2001-09 | Glass-alumina composites prepared by melt-infiltration: I. Effect of alumina particle size | 이득용; 장주웅; 김대준; 박일석; 이준강; 이명현; 김배연 |