dc.description.abstractTo investigate degradation mechanism of PEMFC operated with repetitive startup/shutdown cycling, i-V characteristics, impedance, cyclic voltamograms were measured. OCV decreased from 0.967 to 0.951 V while the cell voltage at 800mA/cm2 from 0.657 to 0.563V, implying that the electrodes rather than membrane electrolyte was damaged during the cycling operation. Electrochemical analyses supported that the performance degradation could be mainly attributed to degradation of the electrodes such as a decrease in electrochemical active surface area rather than degradation of membrane.-
dc.languageKorean-
dc.publisher한국수소및신에너지학회-
dc.title시동/정지 반복에 따른 고분자전해질 연료전지의 성능 저하에 관한 연구-
dc.title.alternativeA Study on Performance Degradation of PEMFC by Repetitive Startup/Shutdown Cycling-
dc.typeArticle-
dc.description.journalClass2-
dc.identifier.bibliographicCitation한국수소및신에너지학회논문집, v.20, no.4, pp.317 - 322-
dc.citation.title한국수소및신에너지학회논문집-
dc.citation.volume20-
dc.citation.number4-
dc.citation.startPage317-
dc.citation.endPage322-
dc.description.journalRegisteredClasskci-
dc.identifier.kciidART001374156-
dc.subject.keywordAuthorPEMFC-
dc.subject.keywordAuthorDegradation-
dc.subject.keywordAuthorStartup/Shutdown-
dc.subject.keywordAuthorDummy load-
dc.subject.keywordAuthor고분자전해질 연료전지-
dc.subject.keywordAuthor열화-
dc.subject.keywordAuthor시동/정지-
dc.subject.keywordAuthor더미 저항-
Appears in Collections:
KIST Article > 2009
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE