Synthesis of homogeneous la0.8Sr0.2CrO3 powders using an ultrasonic spray pyrolysis method
- Authors
- Kim, C.-S.; Hwang, S.I.; Kim, S.W.
- Issue Date
- 2007-05
- Publisher
- Korean Ceramic Society
- Citation
- Journal of the Korean Ceramic Society, v.44, no.5, pp.148 - 150
- Abstract
- A process to synthesize La0.8Sr0.2CrO3 (LSC), which is a promising material for use as a separator in a soild oxide fuel cell, is investigated in this study. LSC powders without secondary phases could be synthesized with ultrasonic spray pyrolysis and a heat treatment at 1200°C for 20 h: however, it showed an average diameter of 0.6 μm with a wide particle size distribution. On the other hand, LSC powders synthesized with spray pyrolysis at 800°C, heat-treated at 900°C for 5 h, ball-milled and finally heat-treated again at 1200°C for 20 h showed a smaller average diameter of 0.3 μm and narrower size distribution. Very few particles above 0.5 μm were found. Thus, a proper combination of the heat treatment and milling process after spray pyrolysis it determined to be very important in synthesizing fine and uniform LSC perovskite powders.
- Keywords
- La0.8Sr0.2CrO3; Separator; Solid oxide fuel cell; Ultrasonic spray pyrolysis
- ISSN
- 1229-7801
- URI
- https://pubs.kist.re.kr/handle/201004/134418
- DOI
- 10.4191/KCERS.2007.44.5.148
- Appears in Collections:
- KIST Article > 2007
- Files in This Item:
There are no files associated with this item.
- Export
- RIS (EndNote)
- XLS (Excel)
- XML
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.