Embrittlement of Pd-Coated Ni-Nb-Ti-Zr Amorphous Alloys during Hydrogen Permeation

Authors
Lee, Dock-YoungFleury, Eric
Issue Date
2008-10
Publisher
KOREAN INST METALS MATERIALS
Citation
METALS AND MATERIALS INTERNATIONAL, v.14, no.5, pp.549 - 552
Abstract
In this study, we report results of an investigation into the failure of Ni60Nb15Ti15Zr10 amorphous alloys occurring during hydrogen permeation performed at 473 K and 573 K. However, the amorphous membrane did not fail during test performed at higher temperatures (673 K and 773 K). The failure of the Pd-coated Ni60Nb15Ti15Zr10 amorphous ribbon is attributed to the cracking of the hydrogenated Pd coating induced by the formation of alpha' hydride phase in the low temperature range.
Keywords
MEMBRANES; MEMBRANES; hydrogen embrittlement; amorphous alloys; melt-spinning; metal membrane
ISSN
1598-9623
URI
https://pubs.kist.re.kr/handle/201004/133106
DOI
10.3365/met.mat.2008.10.549
Appears in Collections:
KIST Article > 2008
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE