Reversible hydrogen storage in LiBH4-Al-LiH composite powder
- Authors
- Jin, Seon-Ah; Shim, Jae-Hyeok; Cho, Young Whan; Yi, Kyung-Woo; Zabara, Oleg; Fichtner, Maximilian
- Issue Date
- 2008-06
- Publisher
- PERGAMON-ELSEVIER SCIENCE LTD
- Citation
- SCRIPTA MATERIALIA, v.58, no.11, pp.963 - 965
- Abstract
- A composite powder has been prepared by ball milling a mixture of LiBH4 and LiAlH4 together with 3 mol.% TiF3. The powder starts to decompose between 450 and 520 K and the weight loss reaches up to 7.2 wt.%. The formation of AlB2 is clearly observed after desorption at 673 K for 4 h. It is also confirmed that dehydrogenated product can be hydrogenated to about 5.1 wt.% H-2 at 623 K for 6 h under 70 bar of hydrogen. (c) 2008 Acta Materialia Inc. Published by Elsevier Ltd. All rights reserved.
- Keywords
- CHEMICAL-REACTION; DESTABILIZATION; DECOMPOSITION; BOROHYDRIDES; LIBH4; CHEMICAL-REACTION; DESTABILIZATION; DECOMPOSITION; BOROHYDRIDES; LIBH4; hydrogen storage; mechanical milling; hydrides; borides; reactive composite
- ISSN
- 1359-6462
- URI
- https://pubs.kist.re.kr/handle/201004/133446
- DOI
- 10.1016/j.scriptamat.2008.01.028
- Appears in Collections:
- KIST Article > 2008
- Files in This Item:
There are no files associated with this item.
- Export
- RIS (EndNote)
- XLS (Excel)
- XML
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.