Electrical transport, magnetic, and electronic structure studies of Mg(0.95)Mn(0.05)Fe(2-2x)Ti2xO4 +/-delta (0 <= x <= 0.5) ferrites
- Authors
- Kumar, Shalendra; Alimuddin; Kumar, Ravi; Thakur, P.; Chae, K. H.; Angadi, Basavaraj; Choi, Wk
- Issue Date
- 2007-11-28
- Publisher
- IOP PUBLISHING LTD
- Citation
- JOURNAL OF PHYSICS-CONDENSED MATTER, v.19, no.47
- Abstract
- We present structural, electrical transport, magnetic, and electronic structure studies of Mg(0.95)Mn(0.05)Fe(2-2)xTi(2x)O(4) ferrite using x-ray diffraction, dielectric spectroscopy, DC magnetization and near edge x-ray absorption fine structure (NEXAFS) measurements. The x-ray diffraction study shows a structural transition from cubic to tetragonal with Ti substitution. The dielectric constant and DC conductivity increase with Ti substitution up to x = 0.2. However, with further increase of substitution both the dielectric constant and DC conductivity decrease. This electrical behavior indicates that at low values of substitution, hopping between Fe3+ and Fe2+ increases whereas at higher concentrations the total content of Fe ions decreases. It is observed that all the samples exhibit ferrimagnetic behavior at 300 K and the saturationmagnetization decreases with increase in Ti substitution. The NEXAFS measurements have been carried out at O K-, Fe L-, Fe K-, and Ti L- edges to investigate the chemical states and the electronic structure of the Mg0.95Mn0.05Fe2-2xTi2xO4 ( 0 <= x <= 0.5) system at room temperature. The O K- edge spectra indicate that the Fe 3d orbitals are considerably modified with the substitution of Ti ions. At x >= 0.3, a new spectral feature appears ( similar to 532 eV) due to the transitions from oxygen 2p to Ti 3d orbitals which starts dominating the pre-edge spectra of the system. Both Fe L-3,L-2- and Fe K-edge spectra indicate that iron Fe3+ ions convert into Fe2+ with the substitution of Ti ions. The Ti L-3,L-2- edge NEXAFS spectra reveal that the Ti remains in the 4+ state for all the samples. The observed experimental results have been explained on the basis of dilution of the magnetic sublattice by Ti substitution, which provides a strong interplay between electrical and magnetic properties along with their electronic structure.
- Keywords
- DIELECTRIC BEHAVIOR; ZN FERRITES; MOSSBAUER; CONDUCTIVITY; TEMPERATURE; TRANSITION; GLASS; DIELECTRIC BEHAVIOR; ZN FERRITES; MOSSBAUER; CONDUCTIVITY; TEMPERATURE; TRANSITION; GLASS; electronic structure; NEXAFS; Ferrite
- ISSN
- 0953-8984
- URI
- https://pubs.kist.re.kr/handle/201004/133970
- DOI
- 10.1088/0953-8984/19/47/476210
- Appears in Collections:
- KIST Article > 2007
- Files in This Item:
There are no files associated with this item.
- Export
- RIS (EndNote)
- XLS (Excel)
- XML
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.