Preparation of polystyrene particles containing poly(ethylene glycol) groups and their surface charge characterization in dielectric medium
- Authors
- Kim, SH; Kim, BJ; Kwon, DI; Park, KH
- Issue Date
- 2004-11
- Publisher
- POLYMER SOC KOREA
- Citation
- POLYMER-KOREA, v.28, no.6, pp.524 - 530
- Abstract
- Polystyrene particles (PS) with poly(ethylene glycol) units on surface were formed by an emulsifier-free emulsion polymerization using styrene, poly(ethylene glycol) methacrylate (PEG-MMA) or poly(ethylene glycol) dimethacrylate (PEG-diMMA) at pH 7, and followed by freeze-drying to give the corresponding powders. The structures of PS particles were confirmed by FT-IR spectroscopy, and the particle size and distribution the PS particle were observed by scanning electron microscopy and particle analyzer. Monodisperse polymer particles were obtained at a concentration of PEG-MMA 2similar to5 mol% or PEG-diMMA 1 mol% relative to styrene. The highest zeta potential of polymer surface was measured to be 183 mV at a polymer of PEG-MMA 5 mol%, which was measured in dielectric medium by means of ELS-8000 dynamic light scattering.
- Keywords
- FREE EMULSION POLYMERIZATION; STYRENE; LATEXES; COMONOMER; MECHANISM; SYSTEM; FREE EMULSION POLYMERIZATION; STYRENE; LATEXES; COMONOMER; MECHANISM; SYSTEM; emulsifier-free emulsion polymerization; poly(ethylene glycol) methacrylate; poly(ethylene glycol) dimethacrylate; polystyrene powders; zeta potential
- ISSN
- 0379-153X
- URI
- https://pubs.kist.re.kr/handle/201004/137108
- Appears in Collections:
- KIST Article > 2004
- Files in This Item:
There are no files associated with this item.
- Export
- RIS (EndNote)
- XLS (Excel)
- XML
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.