- Abstract
- The room temperature wet catalytic oxidation was conducted in a batch reactor with V/MgO catalyst. The XRD study of the catalyst used indicated that V/MgO could not only oxidize H2S to sulfur selectively, but also prevent the sulfidation of metal oxide effectively at room temperature. The XPS study indicated that the H2S oxidation with V/MgO could proceed by a redox mechanism (V5+ <----> V4+) and that V3+ formation (V4+--> V3+), was responsible for the deactivation of V/MgO.
- Keywords
- SELECTIVE OXIDATION; HYDROGEN-SULFIDE; OXIDE CATALYSTS; SULFUR; SELECTIVE OXIDATION; HYDROGEN-SULFIDE; OXIDE CATALYSTS; SULFUR; wet catalytic oxidation; V/MgO catalyst; H2S; redox mechanism
- ISSN
- 0133-1736
- URI
- https://pubs.kist.re.kr/handle/201004/137381
- DOI
- 10.1023/B:REAC.0000037372.59994.f7
- Appears in Collections:
- KIST Article > 2004
- Files in This Item:
There are no files associated with this item.
- Export
- RIS (EndNote)
- XLS (Excel)
- XML
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.