Effect of green density on the subsequent densification and grain growth of ultrafine SnO2 powder during isochronal sintering
- Authors
- Ahn, JP; Park, JK; Huh, MY
- Issue Date
- 1997-08
- Publisher
- WILEY-BLACKWELL
- Citation
- JOURNAL OF THE AMERICAN CERAMIC SOCIETY, v.80, no.8, pp.2165 - 2167
- Abstract
- An ultrafine powder of SnO2 has been synthesized by a gas flow condensation method. The average particle size of the powder was about 40 nm, The effect of the green density on the subsequent densification and grain growth of the ultrafine SnO2 during sintering has been studied. A loose green compact consolidated under 500 MPa (green MC) showed rapid densification as well as rapid grain growth at relatively low sintering temperatures. A dense green compact fabricated under 4.5 GPa (green GC) exhibited a slow increase in the density and almost no grain growth even at high sintering temperatures.
- Keywords
- TIO2; TIO2; green density; nanophase; SnO2; isochronal sintering; densification; grain growth
- ISSN
- 0002-7820
- URI
- https://pubs.kist.re.kr/handle/201004/143694
- Appears in Collections:
- KIST Article > Others
- Files in This Item:
There are no files associated with this item.
- Export
- RIS (EndNote)
- XLS (Excel)
- XML
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.