dc.description.abstractUltrahigh molecular weight polyethylene (PE) solution of concentration of 5 wt% was quenched to room temperature to form gel and spun to form fiber, and the effects of zone-drawing conditions on the tensile properties were investigated. Breaking stress and tensile modulus of drawn gel-spun fiber increased and breaking strain decreased with decreasing heal band speed and with increasing drawing temperature. On the other hand, there was a optimum drawing stress for the maximum draw ratio. Maximum draw ratio up to 26.4 was achieved at the heat band speed, drawing temperature, and drawing stress of 1 mm/min, 128 degrees C, and 20 MPa, respectively. Breaking stress, tensile modulus, and breaking strain of gel-spun fiber drawn at these conditions were 2.63 GPa, 43.3 GPa, and 12.75%, respectively. It was identified that breaking stress and tensile modulus increased with an increase in the draw ratio and fraction of tie molecules. Fraction of tie molecules in this study was 0.1732. This value was about 26% of maximum fraction of tie molecules obtained by the drawing of PE.-
dc.languageKorean-
dc.publisherPOLYMER SOC KOREA-
dc.subjectSTRENGTH NYLON-6 FIBER-
dc.subjectMODULUS POLYETHYLENE-
dc.subjectROOM-TEMPERATURE-
dc.subjectANNEALING METHOD-
dc.subjectENTANGLEMENT CONCEPTS-
dc.subjectMECHANICAL-PROPERTIES-
dc.subjectFILAMENTS-
dc.subjectCAST-
dc.subjectSUPERSTRUCTURE-
dc.subjectDEFORMATION-
dc.titleEffect of zone-drawing conditions on the tensile properties of gel-spun ultrahigh molecular weight polyethylene fiber-
dc.typeArticle-
dc.description.journalClass1-
dc.identifier.bibliographicCitationPOLYMER-KOREA, v.20, no.6, pp.1049 - 1060-
dc.citation.titlePOLYMER-KOREA-
dc.citation.volume20-
dc.citation.number6-
dc.citation.startPage1049-
dc.citation.endPage1060-
dc.description.journalRegisteredClassscie-
dc.description.journalRegisteredClassscopus-
dc.identifier.wosidA1996VY11400016-
dc.identifier.scopusid2-s2.0-21444456085-
dc.relation.journalWebOfScienceCategoryPolymer Science-
dc.relation.journalResearchAreaPolymer Science-
dc.type.docTypeArticle-
dc.subject.keywordPlusSTRENGTH NYLON-6 FIBER-
dc.subject.keywordPlusMODULUS POLYETHYLENE-
dc.subject.keywordPlusROOM-TEMPERATURE-
dc.subject.keywordPlusANNEALING METHOD-
dc.subject.keywordPlusENTANGLEMENT CONCEPTS-
dc.subject.keywordPlusMECHANICAL-PROPERTIES-
dc.subject.keywordPlusFILAMENTS-
dc.subject.keywordPlusCAST-
dc.subject.keywordPlusSUPERSTRUCTURE-
dc.subject.keywordPlusDEFORMATION-
dc.subject.keywordAuthorzone drawing condition-
dc.subject.keywordAuthortensile properties-
dc.subject.keywordAuthorpolyethylene gel fiber-
dc.subject.keywordAuthorgel spinning-
dc.subject.keywordAuthortie molecules-
Appears in Collections:
KIST Article > Others
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE