Abstract
This paper reports on the formation of highly densified piezoelectric thick films of 0.01Pb(Mg1/2W1/2)O-3-0.41Pb(Ni1/3Nb2/3)O-3-0.35PbTiO(3)-0.23PbZrO(3)+0.1 wt% Y2O3+1.5 wt% ZnO (PMW-PNN-PT-PZ+YZ) on alumina substrate by the screen-printing method. To increase the packing density of powder in screen-printing paste, attrition milled nano-scale powder was mixed with ball milled micro-scale powder, while the particle size distribution was properly controlled. Furthermore, the cold isostatic pressing process was used to improve the green density of the piezoelectric thick films. As a result of these processes, the PMW-PNN-PT-PZ+YZ thick film, sintered at 890 degrees C for 2 h, showed enhanced piezoelectric properties such as P-r=42 mu C/cm(2), E-c=25 kV/cm, and d(33)=100 pC/N, in comparison with other reports. Such prominent piezoelectric properties of PMW-PNN-PT-PZ+YZ thick films using bi-modal particle distribution and the CIP process can be applied to functional thick films in MEMS applications such as micro actuators and sensors. (C) 2012 Elsevier Ltd and Techna Group S.r.l. All rights reserved.
Keywords
PARTICLE-SIZE; PZT; CANTILEVER; PACKING; PARTICLE-SIZE; PZT; CANTILEVER; PACKING; Piezoelectric thick film; Screen-printing; Particle size control; Cold isostatic pressing
ISSN
0272-8842
URI
https://pubs.kist.re.kr/handle/201004/128337
DOI
10.1016/j.ceramint.2012.07.068
Appears in Collections:
KIST Article > 2013
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE