Fracture surfaces of Zr-based bulk metallic glasses of various compositions tested in the as-cast and annealed conditions were analyzed using scanning electron microscopy The tougher samples have shown highly jagged patterns at the beginning stage of crack propagation, and the length and roughness of this jagged pattern correlate well with the measured fracture toughness values. These jagged patterns, the main source of energy dissipation in the sample, are attributed to the formation of shear bands inside the sample. This observation provides strong evidence of significant "plastic zone" screening at the crack tip
Keywords
NI-CU-BE; FATIGUE-CRACK-PROPAGATION; AMORPHOUS ALLOY; MECHANISMS; BEHAVIOR; FLOW; DEFORMATION; GROWTH; PLATES; NI-CU-BE; FATIGUE-CRACK-PROPAGATION; AMORPHOUS ALLOY; MECHANISMS; BEHAVIOR; FLOW; DEFORMATION; GROWTH; PLATES; amorphous metal; metallic glass; fracture; fracture surface; shear band
ISSN
0884-2914
URI
https://pubs.kist.re.kr/handle/201004/131492
DOI
10.1557/JMR.2010.0112
Appears in Collections:
KIST Article > 2010
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE