Nanopowders of Ni and Al2O3 were synthesized from 3NiO and 2Al powders by high energy ball milling. Nanocrystalline Al2O3 reinforced composite was consolidated by high frequency induction heated sintering method within 2min from mechanically synthesized powders of Al2O3 and 3Ni. The relative density of the composite was 96%. The average hardness and fracture toughness values obtained were 645 kg/mm(2) and 6.3 MPa m(1/2), respectively. (C) 2009 Elsevier Inc. All rights reserved.
Keywords
FRACTURE-TOUGHNESS; HARD MATERIALS; WC; SYSTEM; ZRO2; FRACTURE-TOUGHNESS; HARD MATERIALS; WC; SYSTEM; ZRO2; Rapid sintering; Composite; Nanophase; Mechanical properties; Ni-Al2O3
ISSN
1044-5803
URI
https://pubs.kist.re.kr/handle/201004/131697
DOI
10.1016/j.matchar.2009.12.001
Appears in Collections:
KIST Article > 2010
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE