Mechanochemical synthesis and pressureless sintering of TiB2-AlN composites
- Authors
- Kim, HJ; Choi, HJ; Lee, JG
- Issue Date
- 2002-04
- Publisher
- AMER CERAMIC SOC
- Citation
- JOURNAL OF THE AMERICAN CERAMIC SOCIETY, v.85, no.4, pp.1022 - 1024
- Abstract
- TiB2-AlN composites have been fabricated by the pressureless sintering of a mechanochemically processed Ti, Al, and BN powder mixture. TiB2-AlN powder was obtained from the mixture of Ti, Al, and BN, which had a composition corresponding to 45.7 wt% TiB2-54.3 wt% AlN, after mechanochemical processing for longer than 24 h. X-ray diffraction and transmission electron microscopy analysis showed that the powder subjected to mechanochemical processing for 60 h consisted of crystallites less than 300 run in size with a disordered crystal structure. TiB2-AlN composites with 95% relative density, a flexural strength of 172 MPa, a fracture toughness of 4.6 MPa(.)m(1/2), a hardness of 12.0 GPa, and an electrical resistivity of 1488 muOmega(.)cm were obtained by pressureless sintering at 1700degreesC for 2 h of the powder subjected to mechanochemical processing for 60 h.
- Keywords
- MECHANICAL-PROPERTIES; MICROSTRUCTURE; DENSIFICATION; CERAMICS; MECHANICAL-PROPERTIES; MICROSTRUCTURE; DENSIFICATION; CERAMICS; mechanochemical synthesis
- ISSN
- 0002-7820
- URI
- https://pubs.kist.re.kr/handle/201004/139637
- Appears in Collections:
- KIST Article > 2002
- Files in This Item:
There are no files associated with this item.
- Export
- RIS (EndNote)
- XLS (Excel)
- XML
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.