Thermoelectric properties of (Bi0.25Sb0.75)(2)Te-3 alloys fabricated by hot-pressing method
- Authors
- Hyun, DB; Hwang, JS; Shim, JD; Oh, TS
- Issue Date
- 2001-03
- Publisher
- SPRINGER
- Citation
- JOURNAL OF MATERIALS SCIENCE, v.36, no.5, pp.1285 - 1291
- Abstract
- Thermoelectric properties of the hot-pressed p-type (Bi0.25Sb0.75)(2)Te-3 alloy were characterized with variation of the hot-pressing temperature and the starting powder size. The roles of the factors which affect the Seebeck coefficient of the hot-pressed (Bi0.25Sb0.75)(2)Te-3 alloy has been elucidated in this study. The donor-like behavior of oxygen could be one of the possible explanations for the higher Seebeck coefficient of the hot-pressed (Bi0.25Sb0.75)(2)Te-3 alloy. Te vacancies formed by mechanical deformation during the powdering process significantly promote the diffusion of second phase Te atoms into their lattice sites so that the matrix Te solubility approaches its equilibrium value at a given temperature in a relatively short length of time. Using the Seebeck coefficient at various hot-pressing temperatures, the micro-phase diagram near the stoichiometric composition of (Bi0.25Sb0.75)(2)Te-3 was evaluated. (C) 2001 Kluwer Academic Publishers.
- Keywords
- BI2TE3; bismuth telluride
- ISSN
- 0022-2461
- URI
- https://pubs.kist.re.kr/handle/201004/140660
- DOI
- 10.1023/A:1004862700211
- Appears in Collections:
- KIST Article > 2001
- Files in This Item:
There are no files associated with this item.
- Export
- RIS (EndNote)
- XLS (Excel)
- XML
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.