Morphology of chemical vapor deposition diamond particles grown at high temperature

Authors
Chae, KWBaik, YJ
Issue Date
1999-07
Publisher
ELSEVIER SCIENCE SA
Citation
DIAMOND AND RELATED MATERIALS, v.8, no.7, pp.1261 - 1266
Abstract
{113} facets and irregular shapes of chemical vapor deposition (CVD) diamond particles are observed at high deposition temperature of 1200 degrees C on Co base substrate. Microwave plasma CVD is used for the diamond deposition with 2 percent of methane in hydrogen under 1.2 x 10(4) Pa (90 Torr). {113} facets form between {100} and {111} facets of diamond particles grown on heterogeneous substrate. This verifies that the condition for the stable {113} facet exists in CVD diamond growth. New small angle boundaries evolve on a flat surface of a growing single crystal diamond particle. Solid segments surrounded by the boundaries look like new grains, whose lattice orientations are misoriented to each other. The misorientation between the solid segments is small initially, but increases as the growth proceeds. Such evolution appears only on the upper particle surface which is parallel to the substrate surface irrespective of the facet index. The formation mechanism of the solid segments is discussed in terms of the lattice misfit within the diamond particle. (C) 1999 Elsevier Science S.A. All rights reserved.
Keywords
113 FACETS; GAS-PHASE; SYSTEM; HABIT; 113 FACETS; GAS-PHASE; SYSTEM; HABIT; {113} facet of diamond; misfit dislocation; residual strain; small angle boundary
ISSN
0925-9635
URI
https://pubs.kist.re.kr/handle/201004/142092
DOI
10.1016/S0925-9635(99)00128-4
Appears in Collections:
KIST Article > Others
Files in This Item:
There are no files associated with this item.
Export
RIS (EndNote)
XLS (Excel)
XML

qrcode

Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.

BROWSE