Thermochromism of rapid thermal annealed VO2 and Sn-doped VO2 thin films
- Authors
- Lee, MH; Kim, MG; Song, HK
- Issue Date
- 1996-12-15
- Publisher
- ELSEVIER SCIENCE SA
- Citation
- THIN SOLID FILMS, v.290, pp.30 - 33
- Abstract
- Stoichiometric VO2 thin films were fabricated on glass substrates by reactive electron-beam evaporation under controlled oxygen pressures. Rapid thermal annealing (RTA) was examined as a promising annealing method to crystallize the as-deposited thin film. An RTA temperature of 400 degrees C and time of 20-30 s were found to be optimum annealing conditions to crystallize the thin films, as confirmed by X-ray diffraction analysis and examining the him thermochromism. VO2 thin films were doped with 1-6 at.% Sn to fabricate V1-xSnxO2 thin films. The Sn-doped VO2 thin films exhibited distinct thermochromism as the undoped thin films, however, they showed significantly higher transition temperatures than undoped VO2 thin films.
- Keywords
- VANADIUM DIOXIDE; OPTICAL-PROPERTIES; TEMPERATURE; TRANSITION; DEPOSITION; OXIDE; VANADIUM DIOXIDE; OPTICAL-PROPERTIES; TEMPERATURE; TRANSITION; DEPOSITION; OXIDE; annealing; vanadium oxide; evaporation
- ISSN
- 0040-6090
- URI
- https://pubs.kist.re.kr/handle/201004/144202
- DOI
- 10.1016/S0040-6090(96)09201-2
- Appears in Collections:
- KIST Article > Others
- Files in This Item:
There are no files associated with this item.
- Export
- RIS (EndNote)
- XLS (Excel)
- XML
Items in DSpace are protected by copyright, with all rights reserved, unless otherwise indicated.